Aluminum grey colour profile

    Model Number: AE50-6063
  • Place of Origin: Guangxi, China
  • Brand Name: Gold Apple
  • Certification: ISO9001, ISO14000, ISO10012
  • Temper: T3-T8
  • Grade: 6000 Series
  • Alloy Or Not: Is Alloy
  • Minimum Order Quantity: 10 tons after confirmed the samples
  • Thickness: >0.7mm
  • Length: 1-8M

Product Details

Aluminum grey colour profile, Competitive price.Alloy and temper: 6061,6063, 6060,6005 or other alloys, temper can be T4/T5/T6 etc.We can manufacture according to your size and shape of such aluminum profile.Our colour is stable , gloss is high .Rich-experience Engineers give you technical and professional suggestion in designing and installation.

construction requirements, general powder spraying construction requirements:

(1) in order to give full play to and extend the service life of the coating, the surface of the coating is strictly treated by surface pretreatment first

(2) when spraying, the coating must be completely ground to increase the spraying efficiency of the powder coating

(3) to be coated with larger surface defects, it should be coated with conductive putty to ensure the smooth and smooth coating

(4) after the spraying, the objects and articles should be heated, cured and cured. The technical indexes of the powder products should be adopted. However, the curing temperature and time should be guaranteed so as to avoid the lack of solidification and cause quality accidents.

(5) check immediately after spraying, if found defects should be timely treatment, if after curing defects are found, the only local small range without affecting, the coated surface decoration, can use the same color powder and acetone diluted to repair, if the scope is large and affects the surface quality, use sandpaper after again. Or use the paint remover to remove the coating, re Suo powder.

(6) the recovered powder must be screened and removed, and then mixed with the new powder at a certain proportion.

(7) the powder supply barrel, the powder spraying room and the recycling system should avoid contamination by other colors. Therefore, each color change must be cleaned.

Factory

Recommended products